Mechanical Properties Metric English Comments
Flexural Yield Strength 115 - 120 MPa

@Temperature 90.0 - 90.0 °C
16700 - 17400 psi

@Temperature 194 - 194 °F
Average value: 118 MPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Flexural Yield Strength 28.0 - 120 MPa
4060 - 17400 psi
Average value: 74.9 MPa Grade Count:14
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Flexural Yield Strength 90.0 - 120 MPa
13100 - 17400 psi
ASTM D790
Chang Chun Plastic PBT2100 Fire Retardant PBT
Information provided by Dowell Trading Company Ltd.
Flexural Yield Strength 120 - 120 MPa

@Temperature 80.0 - 80.0 °C
17400 - 17400 psi

@Temperature 176 - 176 °F
Average value: 120 MPa Grade Count:1
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..