Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 62.1 - 91.7 MPa | 9000 - 13300 psi | Average value: 78.0 MPa Grade Count:26 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Yield Strength | 74.0 - 92.0 MPa | 10700 - 13300 psi | Average value: 81.2 MPa Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |