Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 3.45 - 68.9 MPa | 500 - 10000 psi | Average value: 22.2 MPa Grade Count:32 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 49.0 - 69.0 MPa | 7110 - 10000 psi | Average value: 65.8 MPa Grade Count:13 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Yield Strength | 27.6 - 68.9 MPa | 4000 - 10000 psi | Average value: 52.5 MPa Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Flexural Yield Strength | 62.0 - 69.0 MPa | 8990 - 10000 psi | ASTM D790 |
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet
(discontinued **) Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical.. |
|||
Flexural Yield Strength | 41.4 - 68.9 MPa | 6000 - 10000 psi | Average value: 58.6 MPa Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |