Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
PTS Trimid® N66-S100HL-BK High Impact Heat Stabilized Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 65.5 - 142 MPa | 9500 - 20600 psi | Average value: 104 MPa Grade Count:65 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 65.5 - 255 MPa | 9500 - 37000 psi | Average value: 138 MPa Grade Count:19 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM-D790 |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PBT IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Spartech Royalite R52 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Spartech Royalite R66 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Star Plastics ABS450FR Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Chase Plastics CP Pryme® APC300 ABS Polycarbonate Alloy, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Clariant Renol PPSP0005 Polypropylene Homopolymer, Glass Fiber and Mica Reinforced, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 65.5 MPa | 9500 psi | ASTM D790 |
PlastxWorld CEVIAN® B45M0 PBT/ABS Alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |