Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific) ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy FXTW26SK ASA Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWM206 ASA Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Rotuba H4 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region... |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall Information Provided by LG Chem |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Hannam Chemical Hanalac 750 ABS, General Purpose FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: elect.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp ZP003 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZP003 is a compound based on PPE + PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PVX524 PPE PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific) PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MC004 PP (Europe-Africa-Middle East) LNP* Thermocomp* MC004 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Tipco Tipcolene® FPM 40 - 40% Mica Reinforced Polypropylene Homopolymer, High Stiffness 40% Mica Reinforced PP HomopolymerApplications: Electrical & AutomotiveProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Eastman Tritan LX150HF Copolyester Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades .. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Eastman Tritan MX730 Copolyester Eastman Tritan Copolyester MX730 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX730 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Eastman Tritan MX731 Copolyester Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Eastman Tritan WX500 Copolyester Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet
(discontinued **) USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire c.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Kleerdex Kydex® 150 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Kleerdex Kydex® 550 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable monolithic sheetApplications: Housings for equipment, recreational vehicles and truck parts, safety equipment, building products, signageFeatures: Kydex 550 offers the properties of "Kyd.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY CR7500 ASA High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp FF006 PE LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region. |