Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 585 MPa | 84800 psi | ASTM D790 |
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for ap.. |