Polymer Property : Flexural Yield Strength = 74700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 515 - 1448 MPa

@Temperature 71.0 - 90.0 °C
74700 - 210000 psi

@Temperature 160 - 194 °F
Average value: 967 MPa Grade Count:9
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..