Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 46.9 MPa | 6800 psi | ASTM D790 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 29% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Flexural Yield Strength | 46.9 MPa | 6800 psi | ASTM D790 |
Westlake Plastics Kynar® 2850 PVDF Copolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Flexural Yield Strength | 46.9 MPa | 6800 psi | ASTM D790 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 46.9 - 85.5 MPa | 6800 - 12400 psi | Average value: 64.8 MPa Grade Count:11 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |