Mechanical Properties Metric English Comments
Flexural Yield Strength 40.2 MPa

@Thickness 6.40 mm
5830 psi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL GP3302 PP+MF30%
Description: Injection Molding, PP+MF30%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG..
Flexural Yield Strength 40.2 MPa

@Thickness 6.40 mm
5830 psi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL HI5302A PP+MF15%, High Impact
Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical