Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 4.00 - 75.0 MPa | 580 - 10900 psi | Average value: 34.8 MPa Grade Count:41 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Yield Strength | 4.00 - 4.80 MPa | 580 - 696 psi | |
Struktol MAGNESIUM STEARATE High purity stearate with low soluble salt level that reduces discoloration during processing.STRUKTOL® Magnesium Stearate is used by the rubber and plastic industries as an effective elastomer p.. |