Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 36.0 MPa | 5220 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® INP581 ABS High flow, low molecular weight SAN.
Can be used as compounding additives for polymer blends.
Can be blended with high rubber graft modifier resins to produce customized ABS properties.
Suitable for.. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for.. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Ineos Nova 5810 High Impact Polystyrene
(discontinued **) Balance of toughness and rigidity, Good gloss, USP Class VIApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection .. |
|||
Flexural Yield Strength | 36.0 - 200 MPa | 5220 - 29000 psi | Average value: 139 MPa Grade Count:102 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | At 5% strain |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp FF001 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FF001 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006SXP is a compound based on Polypropylene resin containing Glass Bead. Added featurs include: Heat Stabilized. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MX05039 PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MX05039 is a compound based on Polypropylene resin containing Mineral, colorant. Added features include : Heat- Stabilized, UV - Stabilized.This data was supplied by SABIC-IP for th.. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Tipco Tipcolene® CR 8233 - 20% Talc/Mineral Reinforced Polypropylene Copolymer Compound 20% Mineral Reinforced PP CopolymerApplications: Automotive Pillars & TrimsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Tipco Tipcolene® FPZ-GC - Talc/Mineral Reinforced Polypropylene Copolymer, High Flow, Stiffness & Impact Strength Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | 2 mm/min; ISO 178 |
Eurostar Starglas FF001 HDPE, Glass Fiber Filled Starglas FF001 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | 2 mm/min; ISO 178 |
Eurostar Starpylen MX05039 PP, Mineral Filled, Injection Molding Starpylen MX05039 is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | At 5% strain |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Ineos Nova 4501 Medium Impact Polystyrene
(discontinued **) Good toughnessApplications: Light louvers, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provide.. |
|||
Flexural Yield Strength | 36.0 MPa | 5220 psi | ASTM D790 |
Ineos Nova 5530 High Impact Polystyrene
(discontinued **) Good overall balance of properties, Good toughnessApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C.. |