Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 359 MPa | 52100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East) LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Flexural Yield Strength | 359 MPa | 52100 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Flexural Yield Strength | 359 MPa | 52100 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |