Mechanical Properties Metric English Comments
Flexural Yield Strength 33.1 - 143 MPa
4800 - 20700 psi
Average value: 100 MPa Grade Count:198
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 17% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 17% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 17% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Eastman Tenite Butyrate 530E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Eastman Tenite Butyrate 550E4861316 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Eastman Tenite Butyrate 575E3720010 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Copyright © lookpolymers.com All Rights Reserved