Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 312 MPa
45300 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PF00C is a compound based on PA6 resin containing Glass Fiber.
Flexural Yield Strength 312 MPa
45300 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00CS PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PF00CS is a compound based on PA6 resin containing Glass Fiber.