Polymer Property : Flexural Yield Strength = 3700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 25.5 MPa

@Thickness 6.40 mm
3700 psi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUPOL HI4352L PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9003-07-0, 26221-73-8 and 14807-96-6Inform..
Flexural Yield Strength 25.5 MPa
3700 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 20% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Yield Strength 25.5 MPa
3700 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 20% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Yield Strength 25.5 MPa
3700 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 20% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Flexural Yield Strength 25.5 MPa
3700 psi
ASTM D790
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 20% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..