Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 2830 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 19.5 MPa
2830 psi
ASTM D790
Tipco Tipcolene® TPE-HMI TPE HMI - Impact Modified Polypropylene Copolymer Compound with High Flow, Soft Touch
High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Yield Strength 19.5 MPa
2830 psi
ASTM D790
Tipco Tipcolene® MD-TPE MD TPE - Impact Modified Polypropylene Copolymer Compound for Automobile Bumpers
High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.