Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 158.6 MPa | 23000 psi | ASTM D790 |
PTS Trimid® N6-G30L 30% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | Sheet Stress |
Hardwire 3SX-4-12 Low Density Composite The 3SX Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3SX cord is used where balanced compressive and tensile strengths are required as w.. |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6 GF25 FR IM 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Flame Retardant and Impact ModifierFeatures: Flame Retardant and Impact Modifi.. |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES Luriblend® PC CF15 TL6 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I.. |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES Luriblend® PC GF20 TL10 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, In.. |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES Luriblend® PC GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES Plaslube® J-50/20/TF/10 Polycarbonate, 20% GFR, 10% PTFE |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b.. |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | ASTM D790 |
Westlake Plastics Zelux® 30% GF Polycarbonate 30% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | ASTM D790 |
Clariant Renol PA213G15 Nylon 6, 15% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 159 MPa | 23000 psi | ASTM D790 |
PlastxWorld CEVIAN® S5230 30% GF PC/ABS alloy Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld .. |