Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 157 MPa @Thickness 6.40 mm |
22800 psi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant Feature: Injection Molding, PA6+GF15%, Flame RetardantApplication: ConnectorsCAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN333G15HI Multi Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Yield Strength | 157 MPa @Thickness 3.20 mm |
22800 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2200 PBT+GF20% Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 157 MPa @Thickness 3.20 mm |
22800 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN132G15VO G/F Reinforced Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Yield Strength | 157 MPa @Thickness 3.20 mm |
22800 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2306FY PBT+GF30% Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided .. |
|||
Flexural Yield Strength | 157 MPa @Thickness 3.20 mm |
22800 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® HI2303 PBT+GF30% Description: Injection Molding, PBT+GF30%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon DE002E PC (Europe-Africa-Middle East) LNP* STATKON* DE002E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features include; Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQNH4550 PBT Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% .. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JF003L PES LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r.. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | ASTM D790 |
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WFB44 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WFB44 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Glass Bead. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa.. |
|||
Flexural Yield Strength | 157 MPa | 22800 psi | DIN 53455; ASTM D790 |
Kolon SPESIN® KP213G15 Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |