Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 15.7 - 97.2 MPa | 2280 - 14100 psi | Average value: 35.2 MPa Grade Count:37 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Flexural Yield Strength | 15.7 MPa @Thickness 6.40 mm |
2280 psi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL HF5157Z PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good PaintabilityApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provided by LG Chemical |
|||
Flexural Yield Strength | 15.7 MPa @Thickness 6.40 mm |
2280 psi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi.. |