Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 145 MPa | 21000 psi | ISO 178, ASTM D790 |
Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Asia Pacific) Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East) DATA ON BK1005 ONLY. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS DATA ON BK1005 ONLY. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | ASTM D790 |
Techmer ES Luriblend® PC CF10 TL10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I.. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® SHF4340 PBT 20% GF Super High Flow PBT |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No.. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | ASTM D790 |
Tipco Tipcofil® AG 200 - 10% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 10% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | ASTM D790 |
PlastxWorld CEVIAN® A2604 20% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | ASTM D790 |
Cresset Powers Cress-Alon™ NF3020 2% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, Dry As Molded Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib.. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | 2 mm/min; ISO 178 |
Eurostar Staramide PFB42ES PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42ES is a Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Yield Strength | 145 MPa | 21000 psi | ASTM D790 |
E-Polymers TEKAMID® TB120G15T Impact Modified, 15% Glass Fiber Reinforced PA6, DAM 15% GF reinforced, Good impact resistanceInformation provided by E-Polymers Co. Ltd. |