Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 127 MPa @Thickness 3.20 mm |
18500 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 127 MPa @Thickness 6.40 mm |
18500 psi @Thickness 0.252 in |
1mm/min; ASTM D790 |
LG Chemical LUCON CP510F PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b.. |
|||
Flexural Yield Strength | 127 MPa @Thickness 6.40 mm |
18500 psi @Thickness 0.252 in |
1mm/min; ASTM D790 |
LG Chemical LUCON PN9008 PPS+MF+GF Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212.. |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN126 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Yield Strength | 127 MPa @Thickness 3.20 mm |
18500 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 127 MPa @Thickness 3.20 mm |
18500 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Yield Strength | 127 MPa @Thickness 3.20 mm |
18500 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 127 MPa @Thickness 3.20 mm |
18500 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP3400B(W) PA66+MF40%, General Purpose Feature: Injection Molding, PA66+MF40%, General PurposeApplication: Automotive (Engine Cover)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN3311 General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Yield Strength | 127 MPa @Thickness 3.20 mm |
18500 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 127 MPa @Temperature 23.0 °C |
18500 psi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 330PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN171 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN178MT40 M/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN3311N General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Yield Strength | 127 MPa @Thickness 6.40 mm |
18500 psi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL LW4405 PP+GF/MF40% Description: Injection Molding, PP+GF/MF40%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 65997-17-3 and 12001-26-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | ASTM D790 |
Samyang Trirex® 3025G10 Polycarbonate, 10% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | ASTM D790 |
Cheng Yu Plastic N66C3 Nylon 66, 30% Mineral Reinforced |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | ASTM D790 |
Cheng Yu Plastic N6C2 Nylon 6, 20% Mineral Reinforced |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | ASTM D790 |
Cheng Yu Plastic T882GV1 Flame Retardant PBT, 10% Glass Fiber |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | ASTM D790 |
Cheng Yu Plastic T888G1 PBT, 10% Glass Fiber |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
Clariant Renol PA211G13 Nylon 6, 13% Glass Fiber Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
Clariant Renol PA213G13 Nylon 6, 13% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | ASTM D790 |
Cheng Yu Plastic FRCV150 Flame Retardant Nylon 66, 20% Mineral Reinforced |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 128 - 207 MPa | 18500 - 30000 psi | Average value: 169 MPa Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and.. |
|||
Flexural Yield Strength | 127 MPa @Thickness 3.20 mm |
18500 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Flexural Yield Strength | 127 MPa | 18500 psi | ASTM D790 |
Cheng Yu Plastic ML3410 PC, 10% Glass Fiber |