Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 120 MPa | 17400 psi | ISO 178, ASTM D790 |
Nilit Nilitop BT G2 FR C3 is a 10% Glass Fiber Reinforced, Flame Retardant PBT Description: Nilitop BT G2 FR C3 is a 10% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Asia Pacific) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM XH1015F TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. EFSA food Contact approved. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 500RS PC (Europe-Africa-Middle East) LEXAN 500RS is a medium viscosity, glass reinforced, flame retardant grade. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® DMX3415M PC Copolymer (Europe-Africa-Middle East) Lexan* DMX3415M is a co-polycarbonate resin with improved scratch and abrasion resistance compared to standard polycarbonate. Lexan* DMX3415M is available in transparent colors. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | ASTM D790 |
Lucky EF-940 Acrylic, Injection/Extrusion Grade Extrusion and injection grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capa.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific) This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | ISO 178 |
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | |
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix HexPly® M34 is an epoxy system, specifically developed for low temperature curing of large structural components, particularly in industrial markets. HexPly® M34 is a self-extinguishing system, pr.. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
Eurostar Starglas GX05052 PSU, Glass Fiber Filled Starglas GX05052 is a Glass Fiber Reinforced PSU resin (also known as Starglas PSU A 10V ¾)Information provided by Eurostar. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | ASTM D790 |
E-Polymers TEKAMID® TA210HS , Heat Stabilized PA66, DAM Heat stabilizedInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East) VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 120 MPa | 17400 psi | ASTM D790 |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |