Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 11.7 - 228 MPa | 1700 - 33000 psi | Average value: 118 MPa Grade Count:39 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Flexural Yield Strength | 11.7 MPa | 1700 psi | ASTM D790 |
Clariant Renol 6642 2% Moly Nylon 66, Extrusion Grade, 2% Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |