Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
Lendell Parapet PMMA, High Flow |
|||
Flexural Yield Strength | 108 MPa @Thickness 6.40 mm |
15600 psi @Thickness 0.252 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1300A(W) PA6, High Viscosity Feature: Injection Molding, PA6, High ViscosityApplication: Automotive PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2076F PBT+GF7% Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY ER5151RFA PC/ABS Mineral Filler, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High strength, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 14807-96-6Information p.. |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP2102 PC+GF10% Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP5106F PC/ABS+GF10%, Flame Retardance Description: Injection Molding, PC/ABS+GF10%, Flame RetardanceApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Flexural Yield Strength | 108 MPa @Thickness 3.20 mm |
15600 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5151RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
Samyang Tramid® 210 Polyamide, General Purpose Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210 is a general purpose grade.Applications:Automotive gear level housingConnecto.. |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
Samyang Tramid® 210F Polyamide, High Productivity Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210F is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT.. |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
Samyang Trirex® SF3200GNH20 Polycarbonate, Reinforced Non Halogen for Printers PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.SF3200GNH20 is a reinforced, non-halogen grade for Printers.Applications: Office Machi.. |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
PlastxWorld CEVIAN® S1210 PC/ABS alloy Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
PlastxWorld CEVIAN®-N 050 SAN resin These are typical values and are not intended for specification purposes. UL approved file No. is E47773.Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
Cheng Yu Plastic N66C1 Nylon 66, 10% Mineral Reinforced |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
Cheng Yu Plastic PP237G2 Polypropylene, 20% Glass Fiber |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
Cheng Yu Plastic A700UV ABS-UV Resistance |
|||
Flexural Yield Strength | 108 MPa @Thickness 6.40 mm |
15600 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Flexural Yield Strength | 108 MPa @Thickness 6.40 mm |
15600 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
Cheng Yu Plastic A702G1 ABS 10% Glass Fiber Reinforced |
|||
Flexural Yield Strength | 108 MPa | 15600 psi | ASTM D790 |
PlastxWorld CEVIAN® A5622 10% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |