Mechanical Properties Metric English Comments
Flexural Yield Strength 10.0 - 300 MPa

@Temperature -40.0 - 250 °C
1450 - 43500 psi

@Temperature -40.0 - 482 °F
Average value: 121 MPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Flexural Yield Strength 10.0 - 300 MPa

@Thickness 0.790 - 4.00 mm
1450 - 43500 psi

@Thickness 0.0311 - 0.157 in
Average value: 121 MPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Flexural Yield Strength 10.0 - 207 MPa
1450 - 30000 psi
Average value: 52.0 MPa Grade Count:48
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Flexural Yield Strength 10.0 MPa
1450 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP YP003 Polyester Elastomer (Europe-Africa-Middle East)
LNP* LUBRICOMP* YP003 is a compound based on Polyester Elastomer containing PTFE, Silicone. Added features include; Internally Lubricated.
Copyright © lookpolymers.com All Rights Reserved