Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East) Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East) Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
Flexural Yield Strength | 95.1 MPa | 13800 psi | ASTM D790 |
PolyOne Geon™ CPVC EC050 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC050 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. Geon EC050 demonstrates ease of processing and excellent t.. |
|||
Flexural Yield Strength | 95.1 MPa | 13800 psi | ASTM D790 |
PolyOne Geon™ CPVC EC950 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC950 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC950 demonstra.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7681 PC Copolymer (Asia Pacific) Polycarbonate with high flow, good processability, good impact and thermal properties, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited translucent colors onl.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® PPC4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NS0031 PC+ABS (Asia Pacific) Faradex NS0031 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel. Added features of this material include: EMI/RFI Shiel.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EX2078X PC (Europe-Africa-Middle East) Lexan* EX2078X polycarbonate resin, MVR (300°C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retardant, halogen free per DIN VDE 0472 Part 815, mold release, UV stabilized, translu.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Europe-Africa-Middle East) Lexan LUX9616G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
Flexural Yield Strength | 94.8 - 152 MPa | 13800 - 22000 psi | Average value: 115 MPa Grade Count:7 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Flexural Yield Strength | 95.1 MPa @Thickness 3.20 mm |
13800 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX89795 PC (Europe-Africa-Middle East) LNP* STATKON* DX89795 is a compound based on Polycarbone resin containing Carbon Powder. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp C7410 PC+ABS (Asia Pacific) LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 95.1 MPa | 13800 psi | ASTM D790 |
Samyang Trimma® FT6120 I[R] PMMA, Transparent High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and hi.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX HX7409HP PC+POLYESTER Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA Blowmolding and extrusion. High heat and chemical resistant. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | Plain Cast Resin; ASTM D790 |
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | ASTM D790 |
E-Polymers TEKAMID® TA210HI , High Impact Resistance PA66, DAM High impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Flexural Yield Strength | 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPS6R PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable... |