Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 88.0 MPa | 12800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® FXC1200E PC+ABS (Asia Pacific) Visual Fx PC/ABS for strong fluorescent bright colors with good flow, impact and heat resistance characteristics. Consumer electronic and appliance applications uses. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 3.20 mm |
12800 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUMIPLAS LD590 Light diffusion ABS Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 6.40 mm |
12800 psi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000G PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 24968-12-5 and 103598-77-2Information provid.. |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 6.40 mm |
12800 psi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000GU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info.. |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 6.40 mm |
12800 psi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000SZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 137050-02-03, 26062-94-2 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 3.20 mm |
12800 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 3.20 mm |
12800 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY SC1004A PC Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information.. |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 3.20 mm |
12800 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3020A Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020A is a high flow grade with heat stabilizers.Information provided by Samyang. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3027IR Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3027PU(X) Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PU(X) is an extrusion grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3030U Polycarbonate, UV Stabilized TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 88.0 MPa | 12800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY SLDM2005 PC (Asia Pacific) Antistatic Polycarbonate, Non Halogen FR V-2 grade, mineral 5% filled |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Cheng Yu Plastic SW10 POM/PTFE |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Cheng Yu Plastic VH825 Flame Retardant ABS, Medium Impact |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3020R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020R is a high flow grade with added heat stabilizers and separating materials.Informa.. |