Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 8.20 - 159 MPa | 1190 - 23100 psi | Average value: 88.9 MPa Grade Count:669 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Flexural Yield Strength | 8.20 MPa | 1190 psi | ASTM D790 |
E-Polymers Tekaloy® G70FR , Flame Retardant, Un-Reinforced PC/ABS Alloy Flame Retardant, Impact ResistanceInformation provided by E-Polymers Co. Ltd. |