Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 77.0 MPa | 11200 psi | ASTM D790 |
Plaskolite PETG Mirror Sheet Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® X15 ABS Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS Extrusion blowmolding grade. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS (Asia Pacific) Extrusion blowmolding grade. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | ISO 178 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | ASTM D790 |
Eastman Eastar Copolyester K3000 PETG Copolyester
(discontinued **) EASTAR K3000 Copolyester is a cost effective, high-performance, water-clear material that provides the necessary performance for the appliance standards. Other desirable characteristics are good ch.. |
|||
Flexural Yield Strength | 77.5 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 77.5 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Flexural Yield Strength | 77.5 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 308 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech 513 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech 617 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech 829 Static Conductive Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech Spectar® Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East) LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Europe-Africa-Middle East) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | ISO 178 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Flexural Yield Strength | 77.5 MPa | 11200 psi | ASTM D790 |
Cheng Yu Plastic 3265 TPE Rubber |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Asia Pacific) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
Flexural Yield Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Spartech Spectar® UV Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |