Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® HMG47MD ABS General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG47 ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS Cycoloy MC1300 resin is an injection moldable PC/ABS blend with excellent flow and impact performance. It is designed for plating applications mostly used in the automotive industry. |
|||
Flexural Yield Strength | 72.0 - 86.0 MPa | 10400 - 12500 psi | Average value: 81.1 MPa Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Plenco 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM-D790 |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY MP5000AM PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR474F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific) Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Flexural Yield Strength | 71.7 MPa | 10400 psi | ASTM D790 |
Techmer ES Plastiblend® ABS LG UV Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl EM6100F PPE+PS Automotive interiors. 240F HDT. High impact/good property retention after heat ageing. In blowmolding, better sandability of flash, overblow.This data was supplied by SABIC-IP for the Americas re.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | ASTM D790 |
Eastman Tenite Acetate 105E1R26029 Clear, Trsp Cellulose Acetate TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of TENITE cellulosi.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Flexural Yield Strength | 72.0 MPa @Strain 3.50 % |
10400 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 6.40 mm |
10400 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 72.0 MPa | 10400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP CX94108 PS (Europe-Africa-Middle East) LNP* LUBRICOMP* CX94108 is a compound based on Polystyrene resin containing Proprietary Lubricant. Added features include: Internally Lubricated. |