Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Nylene® Norpex® AX225 HI PPE (Polyphenylene Ether), High Impact Grade Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
PTS Trilac® ABS-HS4000 General Purpose ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
PTS Trilac® ABS-RC3000 Recycled Black ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Faradex AS0029 ABS (Europe-Africa-Middle East) LNP* Faradex* AS-1002 FR is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: Flame Retardant, EM.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® DL100 ABS (Europe-Africa-Middle East) CYCOLAC DL100 is a high heat, high impact, low emissions ABS/PC blend. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Ineos Nova 3500 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill and thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma .. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Ineos Nova 3504 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill an thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma r.. |
|||
Flexural Yield Strength | 68.9 - 147 MPa | 10000 - 21300 psi | Average value: 109 MPa Grade Count:35 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Flexural Yield Strength | 68.9 - 133 MPa | 10000 - 19300 psi | Average value: 103 MPa Grade Count:15 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 68.9 - 260 MPa | 10000 - 37700 psi | Average value: 139 MPa Grade Count:37 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Techmer ES Electrafil® DB-1200/SS/4 ABS, 4% Stainless Steel Fiber Reinforced (dry blend) Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Star Plastics ABS405 Extrusion Grade ABS Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Star Plastics ABSLG3030 Molding Grade ABS, Low Gloss Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12 4.3 specific gravity nylon 12, clean compound system |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman DURASTAR DS1010 Natural PCTA Copolyester DURASTAR DS1010 polymer contains a mold release. It has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to .. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman Eastar AN001 Copolyester, Natural Eastar AN001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman Eastar BR001 Copolyester Eastar BR001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman Eastar Copolyester BR003, Natural PCTA Copolyester EASTAR BR003 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabiliti.. |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 68.9 MPa | 10000 psi | ASTM D790 |
Clariant Renol PCSP0016BL-201 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | Test specimens were injection molded by ASTM D1897; ASTM D790 |
Chevron Phillips K-Resin® BK13 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerBK13 is an SBC developed specifically to have enhanced flow capabilities and improved stiffness over the KR01 grade. BK13 molded parts give excellent detail on rapid prod.. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 5000 is the replacement material for .. |
|||
Flexural Yield Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Plaslok 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound