Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 39.2 - 88.9 MPa | 5690 - 12900 psi | Average value: 72.0 MPa Grade Count:16 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |