Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 70.3 - 230 MPa | 10200 - 33400 psi | Average value: 158 MPa Grade Count:95 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Flexural Yield Strength | 51.7 - 230 MPa | 7500 - 33400 psi | Average value: 142 MPa Grade Count:14 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Yield Strength | 10.3 - 230 MPa | 1500 - 33400 psi | Average value: 123 MPa Grade Count:74 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Flexural Yield Strength | 150 - 230 MPa | 21800 - 33400 psi | ASTM D790 |
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Yield Strength | 150 - 230 MPa | 21800 - 33400 psi | ASTM D790 |
Chang Chun Plastic PBT4130 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |