Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Ravago Manufacturing Americas Hybrid B3030U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 96.5 MPa @Thickness 3.17 mm |
14000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 96.5 MPa @Thickness 3.17 mm |
14000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 96.5 MPa @Thickness 3.17 mm |
14000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 96.5 MPa @Thickness 3.17 mm |
14000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 96.5 MPa @Thickness 3.17 mm |
14000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 96.5 MPa @Thickness 3.17 mm |
14000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 96.5 MPa @Thickness 3.17 mm |
14000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 96.5 MPa @Thickness 3.17 mm |
14000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Yield Strength | 96.5 - 170 MPa | 14000 - 24700 psi | Average value: 129 MPa Grade Count:8 |
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum .. |
|||
Flexural Yield Strength | 96.5 - 117 MPa | 14000 - 17000 psi | Average value: 107 MPa Grade Count:10 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Techmer ES HiFill® ABS HI 0300 High Impact Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Density and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by .. |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Spartech Tuf-Glas Impact Modified Acrylic Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Techmer ES HiFill® PA6 IM 0240 Impact Modified Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Impact ModifierFeatures: High Density and Impact ModifiedProcessing Method: Injection MoldingInform.. |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Techmer ES HiFill® PP GF/M50 CC BK 50% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Techmer ES HiFill® TPX-IONOMER-02045 BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 TS18 Nylon 66 Availability: North AmericaForms: PelletsAdditive: PTFE + Silicone Lubricant (18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Clariant Renol PA2SP0008HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Clariant Renol PA2SP0009HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Clariant Renol PCSP0006GY-371 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 96.5 MPa | 14000 psi | ASTM D790 |
Clariant Renol 6601M Nylon 66, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 96.5 - 124 MPa | 14000 - 18000 psi | |
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound BMC 610 molding compound is a mineral filled, glass fiber reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact.. |