Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 87.8 MPa | 12700 psi | ASTM D790 |
Plenco Valite 759 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4759. Data provided by Plenco.VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and p.. |
|||
Flexural Yield Strength | 87.8 MPa | 12700 psi | DIN 53455; ASTM D790 |
Kolon NOPLA® KE911 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |