Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 76.5 MPa | 11100 psi | DIN 53455; ASTM D790 |
Kolon SPELLOY® KA101 PC + PBT Alloy Resin
(discontinued **) SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional.. |
|||
Flexural Yield Strength | 76.5 MPa @Thickness 3.20 mm |
11100 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI921NS ASA Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Flexural Yield Strength | 76.5 MPa @Thickness 3.20 mm |
11100 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUCON 6080EX ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio.. |
|||
Flexural Yield Strength | 76.5 MPa @Thickness 3.20 mm |
11100 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 76.5 MPa @Thickness 3.20 mm |
11100 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Flexural Yield Strength | 76.5 MPa @Thickness 3.20 mm |
11100 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by .. |
|||
Flexural Yield Strength | 76.5 MPa @Thickness 3.20 mm |
11100 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR490 ABS, Heat Resistance, Low Emission Feature: Injection Molding, Heat Resistance, Low EmissionApplication: Automotives Interior Housing (Glove Box Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG C.. |
|||
Flexural Yield Strength | 76.5 MPa | 11100 psi | ASTM D790 |
Techmer ES Luriblend® TPX-PA6-95002 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 76.5 MPa | 11100 psi | ASTM D790 |
Samyang Tribit® 1700 PBT, Middle Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1700 is a middle viscosity grade.Informatio.. |
|||
Flexural Yield Strength | 76.5 MPa @Thickness 6.40 mm |
11100 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 76.5 MPa @Thickness 6.40 mm |
11100 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 76.5 MPa | 11100 psi | ASTM D790 |
Samyang Tribit® 1800 PBT, High Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1800 is a high viscosity grade.Information .. |
|||
Flexural Yield Strength | 76.5 MPa | 11100 psi | ASTM D790 |
Samyang Triloy® 200 PC/ABS alloy General purposeCharacteristics:Impact resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grill.. |
|||
Flexural Yield Strength | 76.5 MPa | 11100 psi | ASTM D790 |
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |