Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 75.5 MPa @Thickness 3.20 mm |
11000 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HG193S ABS, High Flow, Chemical Resistance Feature: Injection Molding, High Flow, Chemical ResistanceApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 75.5 MPa @Thickness 3.20 mm |
11000 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HI121U ABS Feature: Injection Molding, Well Balanced Mechanical Properties, Good weatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemic.. |
|||
Flexural Yield Strength | 75.5 MPa | 11000 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinblend® A724 PC/PBT, High Impact Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 75.5 MPa | 11000 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinblend® A724 PC/PBT, High Impact Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 75.5 MPa @Thickness 3.20 mm |
11000 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |