Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 72.6 MPa | 10500 psi | 15 mm/min. ASTM D790 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Flexural Yield Strength | 72.6 MPa @Thickness 3.20 mm |
10500 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Flexural Yield Strength | 72.6 MPa @Thickness 3.20 mm |
10500 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 72.6 MPa @Thickness 6.40 mm |
10500 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
LG Chemical TR557 MABS, High Transparency, High Impact Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 72.6 MPa | 10500 psi | ASTM D790 |
IRPC Polimaxx Polene 2511HX GA5 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 25% GLASS FIBRE REINFORCED VERY HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, LOW SHRINKAGE, HIGH STIFFNESS, CONTAIN UV STABILIZER AND LONG TERM.. |
|||
Flexural Yield Strength | 72.6 MPa | 10500 psi | 15 mm/min. ASTM D790 |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Flexural Yield Strength | 72.6 MPa | 10500 psi | ASTM D790 |
Samyang Trimma® SD6350H PMMA, Opaque High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat.. |
|||
Flexural Yield Strength | 72.6 MPa @Thickness 3.20 mm |
10500 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |