Polymer Property : Flexural Yield Strength = 66.38 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 66.38 MPa
9628 psi
ASTM D790
KKPC Kuhmo GP 125EI General Purpose GPPS
Key features: For phonograph, good profile properties. Common Uses: CD-CASE, THIN-WALLGPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding proces..
Flexural Yield Strength 66.38 MPa
9628 psi
ASTM D790
KKPC Kuhmo GP 125 General Purpose GPPS
Key features: Good-fluidity, general purpose. Common Uses: Common kitchenware, toys, general merchandise, cosmetic containers, dust covers.GPPS has excellent transparence, colorability, electric pro..