Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® FXS600AR ABS (Europe-Africa-Middle East) Visual Ares effect Cycolac ABS material with excellent flow properties. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® GX3800F ABS High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® INP581 ABS High flow, low molecular weight SAN.
Can be used as compounding additives for polymer blends.
Can be blended with high rubber graft modifier resins to produce customized ABS properties.
Suitable for.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Flexural Yield Strength | 66.0 - 128 MPa | 9570 - 18600 psi | Average value: 108 MPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® EX58F ABS High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Ineos Nova 1511 High Heat Crystal Polystyrene
(discontinued **) High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Yield Strength | 66.0 - 97.9 MPa | 9570 - 14200 psi | Average value: 90.5 MPa Grade Count:14 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Ineos ABS Cadon® 127 SMA General Purpose, High Heat
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
LG Chemical LG-749 ABS, Low Gloss, High Heat Resistance Information Provided by LG Chem |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Ineos Nova 1510 High Heat Crystal Polystyrene High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Hannam Chemical Hanalac 780 ABS, High Flow FDA Approved. High flow grade suitable for intricate or thin structures and low processing cycle time. Applications include TVs, radios, calculators, appliances, toys. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
KYDEX® 6185 Thermoplastic Sheet High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 364 PBT Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Tritan EX401 Copolyester Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Tritan LX201 Copolyester Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | ASTM D790 |
Eastman Tritan TX2001 Copolyester Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics NORYL FN170X PPE+PS Foamable resin. All properties at 10% density reduction; 0.250"" thick test specimens. |
|||
Flexural Yield Strength | 66.0 MPa | 9570 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |