Polymer Property : Flexural Yield Strength = 585 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 585 MPa
84800 psi
ASTM D790
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC
QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for ap..