Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 538 MPa @Temperature 23.0 °C |
78000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel |