Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 48.3 - 2000 MPa | 7000 - 290000 psi | Average value: 300 MPa Grade Count:182 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Flexural Yield Strength | 48.3 - 280 MPa | 7000 - 40600 psi | Average value: 124 MPa Grade Count:49 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Yield Strength | 48.3 - 110 MPa | 7000 - 16000 psi | Average value: 84.8 MPa Grade Count:6 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Yield Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Spartech Korad® SP-2011 Cap/HIPS Polystyrene Sheet Description: Polystyrene SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
Flexural Yield Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Spartech Royalite R20 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 48.3 MPa | 7010 psi | |
Spartech Royalite R84 Proprietary Polymer Weather Resistant Sheet Data provided by the manufacturer. |
|||
Flexural Yield Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Spartech Royalstatâ„¢ R632 ABS/PVC Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Spartech SP-2010 HIPS Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Spartech SP-2050 Glossy HIPS Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Techmer ES Luriblend® TPX-HDPE-99018 Availability: North AmericaForms: Pellets)Features: Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingTPCI# 8869115Information provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 48.3 MPa | 7000 psi | ASTM D790 |
Westlake Plastics Clariflex® TFE/VF2/HFP Clariflex is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoro-propylene, and vinylidene fluoride. Notable properties include light transmission, chemical resistance.. |
|||
Flexural Yield Strength | 48.3 MPa | 7010 psi | ASTM D790 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Yield Strength | 48.3 MPa | 7010 psi | ASTM D790 |
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Yield Strength | 48.3 MPa | 7010 psi | ASTM D790 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 48.3 MPa | 7010 psi | ASTM D790 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Yield Strength | 48.3 - 80.0 MPa | 7000 - 11600 psi | Average value: 65.6 MPa Grade Count:7 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Flexural Yield Strength | 48.3 MPa | 7010 psi | ASTM D790 |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Yield Strength | 48.3 - 124 MPa | 7000 - 18000 psi | Average value: 94.3 MPa Grade Count:131 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |