Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 448 MPa | 65000 psi | ASTM D790 |
Performance Polymers IPS II PPL-C4270 PEKK (Polyetherketoneketone) Linear 40% Carbon Fiber Reinforced Molding Grade Black pelletsInformation provided by Infinite Polymer System II. |
|||
Flexural Yield Strength | 448 MPa @Temperature 71.0 °C |
65000 psi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel |