Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 40.2 MPa @Thickness 6.40 mm |
5830 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL GP3302 PP+MF30% Description: Injection Molding, PP+MF30%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG.. |
|||
Flexural Yield Strength | 40.2 MPa @Thickness 6.40 mm |
5830 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HI5302A PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |