Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 352 MPa | 51100 psi | ASTM D790 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Yield Strength | 352 MPa | 51100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Flexural Yield Strength | 352 MPa | 51000 psi | ASTM D790 |
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Flexural Yield Strength | 352 MPa | 51000 psi | ASTM D790 |
Techmer ES Plastiblend® PA6/6,6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat.. |