Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 330 MPa | 47900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Opnyl OP66GF60 Nylon 66, 60% Glass Reinforced Nylon 66 - Glass reinforced (60 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared.. |
|||
Flexural Yield Strength | 330 MPa | 47900 psi | ASTM D790 |
Quantum Composites QC-3450 48% Glass Fiber High Temperature Use SMC
(discontinued **) QC-3450 is highly reinforced with glass fibers. It is designed for compression molding of components requiring high structural strength and good resistance to elevated temperatures. Long-term use .. |