Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 27.6 - 68.9 MPa | 4000 - 10000 psi | Average value: 52.5 MPa Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Flexural Yield Strength | 27.6 - 109 MPa | 4000 - 15800 psi | Average value: 48.5 MPa Grade Count:12 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Yield Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Chem Polymer Chemlon 256 Nylon 6, Wire Jacketing Grade A non-halogenated, Allwires rated wire coating grade used primarily on cables for power and control circuits in commercial and industrial applications. The cables are oil, gasoline, and abrasion re.. |
|||
Flexural Yield Strength | 27.6 - 205 MPa | 4000 - 29700 psi | Average value: 90.5 MPa Grade Count:340 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Flexural Yield Strength | 27.6 MPa | 4000 psi | ASTM D790 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 37% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |