Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 246 MPa | 35700 psi | DIN 53452; ASTM D790 |
Kolon Kopa® KN133HB55 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |