Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 164 MPa | 23800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound |
|||
Flexural Yield Strength | 164 MPa | 23800 psi | ASTM D790 |
Cheng Yu Plastic E2325 Flame Retardant PET, 25% Glass Fiber |
|||
Flexural Yield Strength | 164 MPa | 23800 psi | ASTM D790 |
Cheng Yu Plastic E2315 Flame Retardant PET, 15% Glass Fiber |